When repair welding of the O1 tool steel in hardened and tempered condition, the steel should be preheated to a minimum tempering temperature of 200°C (93°F) and welded at the same tempering ...
As stated above, many of the tool steel grades will air harden when air cooled from austenitising temperatures. Annealing Heat Treatment The full annealing heat treatment process involves heating the ...